China Flat Shape Pvb Interlayer Film Clear Heat Resistant for sale
China Flat Shape Pvb Interlayer Film Clear Heat Resistant for sale

Flat Shape Pvb Interlayer Film Clear Heat Resistant

Interlayer Pvb Film Price With Good Quality Product introduction: PVB interlayer is translucent membrance,by polyvinyl butyral resin after plasticizing extrusion forming of a kind of polymer material.Appearance as semi-transparent film,without impurities,with smooth surface,has a certain roughness and good softness,with inorganic glass has good adhesive power,transparent,heat- resistant,cold resistant,resistant to wet and mechanical strength highercharacteristic,It is the

Place of Origin CHINA
Shape Flat
Packaging Details 25kgs/ woven bag or as per customer's request
Color Clear
Model Number Architectural
Supply Ability 500 tons per month
Product Description

Interlayer Pvb Film Price With Good Quality

 

Product introduction:

PVB interlayer is translucent membrance,by polyvinyl butyral resin after plasticizing extrusion forming of a kind of polymer material.Appearance as semi-transparent film,without impurities,with smooth surface,has a certain roughness and good softness,with inorganic glass has good adhesive power,transparent,heat- resistant,cold resistant,resistant to wet and mechanical strength highercharacteristic,It is the world manufacturing laminated,safety glass which widely used to be the best adhesive materials in building curtain wall,recruit,window,bank counter,prison tent out of Windows,and various kinds of bulletproof glass furances screen,and other areas of the building.

 

The main technical parameter of product:

Density 1.069/cm³
Transmittance ≥88.5%
Refractive Index 1.47-1.50
Tensile Stre ≥20Mpa
Elongation at break ≥200%
Moisture  0.35-0.55%
Ration of shrinkage <6%
Test of strike 3-9
Deviation of width Expected value + 10 mm


Note:

1. Measurement under conditions of Colorless glass (2mm) + interlayer film (0.38mm) + Colorless glass(2mm).

2. Measurement under conditions of 20℃ and 40% relative humidity.

3. It is be able to adjust according to cusomers' requirements.

4. Measurement after 15 minutes under the conditions of 60℃ and 40% relative hunmidity.

5. The date of interlayer film of HI (Automotive windshields) and ST (Architectural glass) are different,both samples should be tested with -18℃ after 1 hours.
 

 